Powder Metallurgy of Superalloys details the advancement of powder metallurgy in the context of producing superalloys. The book is comprised of nine chapters that cover the underlying principles of superalloys produced through powder metallurgy. The text first covers concerns in pre-alloyed dispersion-free powders, such as powder production and characterization; powder consolidation methods; and quality control and non-destructive evaluation of P/M superalloys. The next chapter talks about oxide-dispersion-strengthened superalloys. Next, the book discusses joining techniques for P/M superalloys and the practical applications of P/M superalloys. The title will be of great use to professionals in the materials manufacturing industry.
Powder Metallurgy of Superalloys details the advancement of powder metallurgy in the context of producing superalloys. The book is comprised of nine chapters that cover the underlying principles of superalloys produced through powder metallurgy. The text first covers concerns in pre-alloyed dispersion-free powders, such as powder production and characterization; powder consolidation methods; and quality control and non-destructive evaluation of P/M superalloys. The next chapter talks about oxide-dispersion-strengthened superalloys. Next, the book discusses joining techniques for P/M superalloys and the practical applications of P/M superalloys. The title will be of great use to professionals in the materials manufacturing industry.

Front Cover 1
Powder Metallurgy of Superalloys 4
Copyright Page 5
Table of Contents 10
Dedication 6
Preface 8
Foreword 12
Foreword 14
Part 1: Introduction 16
Chapter 1. Introduction 18
1.1. Structure and chemistry of superalloys 18
1.2. Historical development of superalloys 22
1.3. Historical development of powder metallurgical techniques in superalloys 24
Part II: Pre-alloyed dispersion-free powders 32
Chapter 2. Powder production and characterization 34
2.1. Pre-alloyed powders with 'normal' solidification rates 34
2.2. Physical metallurgy of pre-alloyed powders 50
2.3. Alloy development considerations for pre-alloyed powders 55
2.4. Defect control and defect removal in pre-alloyed powders 57
2.5. Pre-alloyed powders with 'rapid' solidification rates (RSR powders) 64
Chapter 3. Powder consolidation methods 74
3.1. Cold compaction and sintering (conventional powder metallurgy) 74
3.2. Hot consolidation techniques 83
3.3. Theories of hot consolidation of powders 95
3.4. Forging of fully dense preforms 104
3.5. Direct melt-solid conversion techniques 112
3.6. Dynamic compaction 122
Chapter 4. Thermomechanical processing principles 127
4.1. Microstructural parameters in superalloys 127
Chapter 5. Mechanical properties of dispersoid-free P/M superalloys 147
5.1. Effect of powder microstructure on microstructure and mechanical properties of consolidated material 147
5.2. Effects of minor alloying elements on mechanical properties 149
5.3. Effects of microstructure on static mechanical properties 156
5.4. High-temperature low-cycle fatigue (HTLCF) 180
5.5. High-temperature fatigue crack growth and creep crack growth 197
Chapter 6. Quality control and non-destructive evaluation of P/M superalloys 217
6.1. Introduction 217
6.2. NDE and quality control of new components 218
6.3. Evaluation of remaining life 221
Part III: Oxide-dispersion-strengthened superalloys 226
Chapter 7. Oxide-dispersion-strengthened superalloys 228
7.1. Introduction 228
7.2. Strengthening mechanisms 229
7.3. Powder production 247
7.4. Powder consolidation 252
7.5. Thermomechanical processing 256
7.6. Mechanical properties 273
7.7. Oxidation and hot corrosion 295
7.8. Development trends for ODS superalloys 301
Part IV: Joining 308
Chapter 8. Joining techniques for P/M superalloys 310
8.1. Liquid-phase bonding 310
8.2. Solid-state bonding 321
8.3. Transient liquid-phase 330
8.4. Applications 332
Chapter 9. Practical applications and economic aspects of P/M superalloys 343
Appendix 1: Nominal composition of superalloys 353
Appendix 2: Registered trademarks and associated companies 357
Appendix 3: Abbreciations used in the text 358
Index 360

Erscheint lt. Verlag 22.10.2013
Sprache englisch
Themenwelt Technik Maschinenbau
Wirtschaft
ISBN-10 1-4831-9244-X / 148319244X
ISBN-13 978-1-4831-9244-4 / 9781483192444
Haben Sie eine Frage zum Produkt?
PDFPDF (Adobe DRM)
Größe: 38,2 MB

Kopierschutz: Adobe-DRM
Adobe-DRM ist ein Kopierschutz, der das eBook vor Mißbrauch schützen soll. Dabei wird das eBook bereits beim Download auf Ihre persönliche Adobe-ID autorisiert. Lesen können Sie das eBook dann nur auf den Geräten, welche ebenfalls auf Ihre Adobe-ID registriert sind.
Details zum Adobe-DRM

Dateiformat: PDF (Portable Document Format)
Mit einem festen Seiten­layout eignet sich die PDF besonders für Fach­bücher mit Spalten, Tabellen und Abbild­ungen. Eine PDF kann auf fast allen Geräten ange­zeigt werden, ist aber für kleine Displays (Smart­phone, eReader) nur einge­schränkt geeignet.

Systemvoraussetzungen:
PC/Mac: Mit einem PC oder Mac können Sie dieses eBook lesen. Sie benötigen eine Adobe-ID und die Software Adobe Digital Editions (kostenlos). Von der Benutzung der OverDrive Media Console raten wir Ihnen ab. Erfahrungsgemäß treten hier gehäuft Probleme mit dem Adobe DRM auf.
eReader: Dieses eBook kann mit (fast) allen eBook-Readern gelesen werden. Mit dem amazon-Kindle ist es aber nicht kompatibel.
Smartphone/Tablet: Egal ob Apple oder Android, dieses eBook können Sie lesen. Sie benötigen eine Adobe-ID sowie eine kostenlose App.
Geräteliste und zusätzliche Hinweise

Buying eBooks from abroad
For tax law reasons we can sell eBooks just within Germany and Switzerland. Regrettably we cannot fulfill eBook-orders from other countries.

Mehr entdecken
aus dem Bereich
Technologie - Berechnung - Klimaschutz

von Volker Quaschning

eBook Download (2023)
Carl Hanser Verlag GmbH & Co. KG
CHF 38,95